Filament Winding

This process involves winding resin-impregnated fiber material around a ‘mandrel’ to create composite products which are typically cylindrical, but can be conical or spherical in shape. Prior to winding, the fiber material is impregnated with the resin system. The deposition angle of the fiber material plays an important role in the final properties of the composite structure.

Applications

  • Pressure Vessels
  • Tanks
  • Drive shafts

Advantages

  • Direct placement of fibers
  • Optimized fiber orientation in load direction
  • Controlled fiber content
  • High laminate quality

 


Product Viscosity
Cps/77°F
Gel Time
Mins/°F
Tg
DSC/DMA/°F
Features
Araldite LY 1564 / Aradur 2954 200 – 300 1 hr / 176 + 8 hrs / 284 294 – 317 Low viscosity / High temperature resistance
Araldite LY 1556 / Aradur 917 /
Accelerator DY 070
700 4 hrs / 176 + 4 hrs / 302 302 – 310 Intermediate temperature use
Araldite LY 1556 / Aradur 906 /
Accelerator DY 070
2000 2 hrs / 248 + 8 hrs / 320 + 2 hrs / 356 340 – 350 High temperature use
RenLam LY 5210 /Aradur 2954 650 – 850 2 hrs / 176 + 2 hrs / 320+ 4 hrs / 356 392 – 400 High temperature resistance / Excellent fiber wet-out